FRACTOGRAPHY ANALYSIS OF INCONEL 718 FATIGUED AT 700°C Journal title: Production Engineering Archives Authors: Michal Jambor, Juraj Belan, Otakar Bokůvka, František Nový Subject(s): Engineering, Educational Technology, Mechanical Engineering