Abstract

Statement of the Problem: The clinical success of ceramic depends on the quality of the bond between the zirconia and resin cement. Purpose: In the present study, the effects of universal and conventional MDP-containing primers were evaluated on the shear bond strength of zirconia ceramic and nanofilled composite resin. Materials and Method: Thirty blocks of zirconia ceramic (6mm×2mm) were prepared. Then the inner surfaces were air-abraded and divided into three groups (n= 10) as follows: untreated with primer (control group, I); All- Bond Universal (group II) and Z-Prime Plus (group III). The specimens in each group were bonded with Variolink N cement to cylinders of composite resin Z350XT. After 24 hour water storage, the shear bond strength test was performed with a universal testing machine at a crosshead speed of 1mm/ min and bond strength values (MPa) were calculated and analyzed with one-way ANOVA and post hoc Tukey tests (p< 0.05). The failure mode of each specimen was evaluated under a stereomicroscope and representative specimens were analyzed by scanning electron microscopy (SEM). Results: The mean shear bond strength values (MPa) were 7.58±1.62, 17.51±1.34 and 22.45±3.60 in groups I, II and III, respectively. These results indicated that the shear bond strength were significantly higher in groups II and III compared to the control group (p< 0.001). Chemical pre-treatment of zirconia with Z- Prime Plus revealed significantly higher bond strength than the All-Bond Universal adhesive (p< 0.002). All the failure modes were adhesive in the control group (I) and when using primer treatment, mixed failures occurred in 40% and 50% of specimens in groups II and III, respectively. Conclusion: Treatment with both primers resulted in higher bond strength values compared to the control group. The use of Z-Prime Plus treatment in combination with air-abrasion procedure resulted in the highest bond strength.

Authors and Affiliations

Farahnaz Sharafeddin, Soodabe Shoale

Keywords

Related Articles

Fear of Falling in Patients with Chronic Stroke: Differences of Functional Gait and Balance Measures According to the Level of Concern about Falling

Background: In this study we investigated the differences of functional gait and balance measures between patients with chronic stroke with different level of concern about falling. Methods: Fifty-four patients with chro...

Comparison of Phonemic Fluency Test Results Using Different Letters among Persian Speakers

Background: The purpose of this study was to compare the results obtained from phonemic fluency test using “F”1, “A”2, “S”3 and “L”4, “T”5,”M”6 among Persian Speakers aged between 20 and 30 years. Methods: In this applie...

Standardization of Connor-Davidson Resilience Scale in Iranian subjects with Cerebrovascular Accident

Background: Resilience is a personal trait that can influence the stroke subjects’ attitudes toward future opportunities and facilitate the transitional process and adaptation in them. Assessment of this trait in stroke...

Effects of Acute Fatigue of the Tibialis Anterior Due to a Weight-Bearing Muscle Activity on the Ankle Joint Position Sense in Healthy Subjects

several sources, including skin, joint capsule/ligaments, and muscular receptors. If the muscle receptors play a leading role in detecting joint position awareness, then muscle fatigue might yield a declination in JPS. T...

Comparison the Pain Relief of Amitriptyline Mouthwash with Benzydamine in Oral Mucositis

Statement of the Problem: A significant proportion of patients undergoing chemotherapy or radiotherapy suffer from mucositis. The first symptom of oral mucositis is pain. Severe pain, burning sensation, and discomfort in...

Download PDF file
  • EP ID EP266251
  • DOI -
  • Views 79
  • Downloads 0

How To Cite

Farahnaz Sharafeddin, Soodabe Shoale (2018). Effects of Universal and Conventional MDP Primers on the Shear Bond Strength of Zirconia Ceramic and Nanofilled Composite Resin. Journal of Rehabilitation Sciences and Research, 19(1), 48-56. https://europub.co.uk/articles/-A-266251