Factors Leading to Major Casting Defects and their Influence on Productivity of Foundry

Abstract

In recent times, with the constant utilization of natural resources, every manufacturing unit is turning towards a lean approach. Foundries are no exception to this. Although the fundamental responsibility of a foundry is simply to convert raw metal into a useful casting, it is imperative on their part that the output confirms with the quality as desired and is free from defects of any kind. However, there may be factors like the rate of cooling of molten metal being poured, mould properties, metallurgy of the molten metal being poured and the mould geometry and rigidity to name a few which may have their influence on the casting quality and the overall productivity of the foundry. While striking a balance between the quality and productivity, there may be certain deviations undertaken from the regular course that may lead to casting defects. This paper intends to highlight such interdependencies and suggest indirectly the most feasible means to control casting defects in order to ensure attainment of both quality and productivity. Casting defects considered for this work shall be those observed at a major scale and those which require adequate attention on account of frequency of occurrence. A conclusion shall be drawn towards the end dictating the major findings of the study. Gourav Vivek Kulkarni "Factors Leading to Major Casting Defects and their Influence on Productivity of Foundry" Published in International Journal of Trend in Scientific Research and Development (ijtsrd), ISSN: 2456-6470, Volume-4 | Issue-6 , October 2020, URL: https://www.ijtsrd.com/papers/ijtsrd35722.pdf Paper Url: https://www.ijtsrd.com/engineering/mechanical-engineering/35722/factors-leading-to-major-casting-defects-and-their-influence-on-productivity-of-foundry/gourav-vivek-kulkarni

Authors and Affiliations

Gourav Vivek Kulkarni

Keywords

Related Articles

Medicine and its Epistemological shift of body of Knowledge: Critical View from Socio-Philosophical Perspectives

The medicine represents a specific type of knowledge about the human body that is applied to either care for or cure of the recipient of medical attention . The nature of medicine is certainly an achieve importance facin...

Evaluation of the Quality of a Prognosis for an Industrial Product using the Regression Analysis

The present research presents the results obtained from a practical study with respect to the evaluation of the quality of a forecast for an industrial product using the regression analysis. A 95 reliability and a 5 erro...

Factor Influencing Post Discharge Care of Hospitalized Children at Home Among Parents

Children are the future resources of the nation. Preservation of their lives will always be a priority. Today lifestyle, environmental and other factors makes the child sick for that they need special treatment. After ho...

A Study for Developing a Microfinance Product in India

Microfinance is a sort of banking services given to people1 with low income, who generally would have no different access to financial services. The objective of Microfinance is to eventually offer the individuals the ch...

GUDUCHI Tinospora Cordifolia The Amrita for Life

Tinospora Cordifolia is a climbing shrub belongs to family Menispermaceae. It is commonly known as Guduchi, Amrita, Gurach, Tinospora. Known by many names in Sanskrit such as gaduchi and Kundalini and scientifically call...

Download PDF file
  • EP ID EP690823
  • DOI -
  • Views 107
  • Downloads 0

How To Cite

Gourav Vivek Kulkarni (2020). Factors Leading to Major Casting Defects and their Influence on Productivity of Foundry. International Journal of Trend in Scientific Research and Development, 4(6), -. https://europub.co.uk/articles/-A-690823