FINDING THE POROSITY PERECENTAGE FOR SMART ALLOY (Cu-Al-Ni) SAMPLES WHEN CHANGING THE SINTERING TIME AT THE FIRST STAGE

Abstract

In this research the effect of porosity is studied at three different holding times(1.5, 1 and 0.5 hours) for the first sintering stage, to fixing aluminium in its solid state phase at temperatures (500°C), of the memory alloy based on copper. The powder metallurgy method has been used to manufacture 3 samples for this alloy with(83%Cu,13%Al,4 %Ni). To make sure of the generation phases for Marten site and Austenite, physical tests (Optical microscopy, XRD, and SEM) were carried out before and after sintering. The porosity testing was conducted on these samples, depending on the specification (ASTM B 328). The percentage of porosity is generated at the three holding times for the first stage was calculated, according to the equation adopted that. The results give, the lowest porosity% was at 0.5 hours with a value of 2.907 %, at 1.5 hours was the highest value for porosity 3.733%, at either hour the value of porosity was 3.720%. In this way we observe the effect of the holding time of the first stage of sintering on the porosity. The relationship was a positive, the greater the holding time, it gives a greater percentage of porosity. It gives an indication of the utilization of those in the process of sintering to obtain the required percentage of porosity, especially in products that need it, such as self-lubricating bearings

Authors and Affiliations

AHMED ABDULRASOOL AHMED ALKHAFAJI

Keywords

Related Articles

Buckling Analysis of Stiffened Composite Panels for Different Ply Orientations

Buckling and post-buckling analysis was performed on composite stiffened panel using Abaqus/CAE to obtain the critical load and modes of failures, with different parameters like ply orientation, different composite mater...

Review on Electric Vehicles

The world wide determination to switch from pollution causing conventional automobiles that run on fossil fuels, to electric vehicles which are pollution free that function with electric power supply drawn from renewable...

Design and Implementation of an Architecture for a Remotely Operated PLC Laboratory Using Labview

In India, imparting practical knowledge about industrial automation to engineering students is still in its infancy. Technical facilities are available only at a few engineering colleges. As a result, it is necessary to...

Hydrofracture Properties via Signals from Hydraulic Pumps: an Overview

Huge water powered breaking is utilized to upgrade creation from the low porous diatomite fields of Kern County, CA. Albeit discriminating for outlining infusion and recuperation well examples, the in-situ pressure drive...

Design and Optimal Synthesis of Compliant Mechanisms– an Optimality Criteria Approach

Compliant mechanisms can be viewed as a single elastic continuum and gain mobility from the deflection of flexible members rather than links and Joints. Compliant Mechanisms are modeled using the methods of continuum sol...

Download PDF file
  • EP ID EP430421
  • DOI 10.24247/ijmperdoct201820
  • Views 77
  • Downloads 0

How To Cite

AHMED ABDULRASOOL AHMED ALKHAFAJI (2018). FINDING THE POROSITY PERECENTAGE FOR SMART ALLOY (Cu-Al-Ni) SAMPLES WHEN CHANGING THE SINTERING TIME AT THE FIRST STAGE. International Journal of Mechanical and Production Engineering Research and Development (IJMPERD ), 8(4), 161-172. https://europub.co.uk/articles/-A-430421