The possibility of vertical take-off of an aircraft is a valuable feature in air transport. It allows to increase operational characteristics of an air vehicle and requires less field and low cost ground infrastructure....
EP ID EP71030
DOI 10.5604/12314005.1134119
Views 84
Downloads 0
How To Cite
Krzysztof Dudzik, Adam Charchalis (2014). FRACTOGRAPHY ANALYSIS OF AW-7020 ALLOY JOINTS WELDED BY FSW. Journal of KONES, 21(1),
67-74. https://europub.co.uk/articles/-A-71030
Sign In Europub
For faster login or register use your social account.
A METHOD OF INVESTIGATING INTERNAL LEAKAGES IN AIRCRAFT HYDRAULIC UNITS
DETERMINATION OF THE TOTAL EFFICIENCY FOR ENGINE WITH SPARK-IGNITION AND COMPRESSION-IGNITION
EXHAUST EMISSIONS OF DUAL FUEL SPARK IGNITION ENGINE FUELLED GASOLINE AND METHANOL
Al2O3 SEALING ELEMENTS LAPPING
A CONCEPTION OF VERTICAL TAKE-OFF AIR VEHICLE WITH SELF-ALIGNING MOVING WINGS
The possibility of vertical take-off of an aircraft is a valuable feature in air transport. It allows to increase operational characteristics of an air vehicle and requires less field and low cost ground infrastructure....