Simulation Segregaton in CMSX-4 Superalloy: Experiments and Simulation Predictions

Journal Title: Jurnalul Stiintific TURBO - Year 2017, Vol 4, Issue 1

Abstract

The segregation degree of alloying elements during solidification in as-cast CMSX-4 singlecrystal superalloy was investigated. The elemental partition coefficients calculated using the results of experimental measurements of local compositions and predicted by thermodynamic calculation in multicomponent alloys have shown the tendency of the elements to segregate either into the dendrites (W, Re) or in the interdendritic regions (Al, Ti, and Ta). Among the alloying elements Re has the strongest tendency to segregate. It was found a good agreement between the experimental and simulation prediction results, as well as compared with an analytical model. By thermodynamic calculation it was established the influence of superalloy chemistry on the elemental segregation during solidification.

Authors and Affiliations

Gheorghe MATACHE, Alexandru PARASCHIV, Cristian PUSCASU, Mihaela Raluca CONDRUZ

Keywords

Related Articles

HEAT TREATMENT INFLUENCE ON HARDNESS AND MICROSTRUCTURE OF ADAM MANUFACTURED 17-4 PH

The influence of heat treatment on the main characteristics of atomic diffusion additive manufactured 17-4 PH stainless steel was studied. Several investigations such as chemical micro-composition, porosity analysis, mic...

Overview of the first Romanian social surveys on aircraft noise annoyance

It is no longer a “taboo” that people who are exposed to long-term noise may experience annoyance as well as health problems. The European Union has tackled this problem with the introduction of the Directive on Environm...

Numerical simulations of pulse combustion in Schubert pulsejet engines

Currently, there is no mathematical model or procedure for designing a pulsejet engine that provides sufficient accuracy to be used in practice. For this reason, the paper addresses the problem by achieving a CFD study o...

Behaviour of a wireless connection during traffic conditions within an industrial environment

The paper describes a Wi-Fi equipment hardware configuration intended for testing of a remote communication system with a terminal, which is part of an automation system belonging to a test bench. The experimentation of...

Self-healing efficiency for fiber reinforced polymer composites

The paper presents a study on self-healing behaviour of fibre reinforced composite materials integrating dicyclopentadiene filled urea-formaldehyde microcapsules as healing system and Grubb’s catalyst as reaction catalys...

Download PDF file
  • EP ID EP268864
  • DOI -
  • Views 148
  • Downloads 0

How To Cite

Gheorghe MATACHE, Alexandru PARASCHIV, Cristian PUSCASU, Mihaela Raluca CONDRUZ (2017). Simulation Segregaton in CMSX-4 Superalloy: Experiments and Simulation Predictions. Jurnalul Stiintific TURBO, 4(1), 11-14. https://europub.co.uk/articles/-A-268864