The structure of Ti-6Al-4V alloy and Ti-6Al-4V weldments was examined. The welds were produced by hollow cathode arc discharge in vacuum using tantalum cathodes and different welding parameters. The corrosion behaviour of Ti-6Al-4V alloy and Ti-6Al-4V welds in solution containing Br- was evaluated quantitatively using potentiodynamic polarization tests. The corrosion behaviour of the base metal and welds was compared. Open circuit potential, pitting potential, corrosion current densities and corrosion rates were determined. The influence of the structure and its change during welding on corrosion behaviour is discussed in the present paper.

Authors and Affiliations

Nikolay Vasilev Ferdinandov, Danail Dimitrov Gospodinov, Mariana Dimitrova Ilieva, Rossen Hristov Radev

Keywords

Related Articles

In-situ modified antimony-film glassy carbon electrode for metal trace analysis

Glassy carbon electrodes (GCE) have been extensively employed for the determination of trace amounts of heavy metals. Lately, modifications of GCE are currently being sought. One way of obtaining better analytical perfor...

New products based on essential oils for finishing natural leathers with antifungal performances – part 2

Research aims the replacement of potentially toxic biocides with ecologic materials – essential oils extracted from plants. Some biocides used in the leather industry have a certain toxicity, and are prohibited by the d...

Dynamic vulcanized thermoplastic elastomers based on ethylene-propylene terpolymer and polyethylene

The paper presents the studies on the obtaining and characterization of new types of dynamically vulcanized thermoplastic elastomers based on ethylene-propylene terpolymer rubber and polyethylene. As a vulcanizing agent,...

Tissue engineering - collagen sponge dressing for chronic wounds

The high number of available wound dressing materials as well as the scientific reports about the topic indicate that the problem of an ideal wound dressing is to be solved. For the last half of century many scientific r...

Study regarding the development of the functional textiles with antimicrobial properties

The antimicrobial fibres, with encapsulated antimicrobial agents, prevent the bacteria developing and maintain the body under hygienic conditions a longer time, refreshing and facilitating the skin respiration, eliminati...

Download PDF file
  • EP ID EP603054
  • DOI 10.24264/icams-2018.VI.7
  • Views 152
  • Downloads 0

How To Cite

Nikolay Vasilev Ferdinandov, Danail Dimitrov Gospodinov, Mariana Dimitrova Ilieva, Rossen Hristov Radev (2018). Structure and pitting corrosion of Ti-6Al-4V alloy and Ti-6Al-4V welds. Proceedings of the International Conference on Advanced Materials and Systems (ICAMS), 1(), 325-330. https://europub.co.uk/articles/-A-603054