Study of verification and validation of standard welding procedure specifications guidelines for API 5L X-70 grade line pipe welding

Journal Title: Журнал інженерних наук - Year 2017, Vol 4, Issue 2

Abstract

Verification and validation of welding procedure specifications for X-70 grade line pipe welding was performed as per clause 8.2, Annexure B and D of API 5L, 45th Edition to check weld integrity in its future application conditions. Hot rolled coils were imported from China, de-coiling, strip edge milling, three roller bending to from pipe, inside and outside submerged arc welding of pipe, online ultrasonic testing of weld, HAZ and pipe body, cutting at fixed random length of pipe, visual inspection of pipe, Fluoroscopic inspection of pipe, welding procedure qualification test pieces marking at weld portion of the pipe, tensile testing, guided bend testing, CVN Impact testing were performed. Detailed study was conducted to explore possible explanations and variation in mechanical properties, WPS is examined and qualified as per API 5L 45th Edition.

Authors and Affiliations

H. A. A. Qazi

Keywords

Related Articles

Implementation of Efficient Artificial Neural Network Data Fusion Classification Technique for Induction Motor Fault Detection

Reliability measurement and estimation of an industrial system is a difficult and essential problematic task for control engineers. In this context reliability can be described as the probability that machine network wil...

Visual object-oriented technology and case-tools of developing the Internet / Intranet-oriented training courses

New information technologies, modern computers, LAN, WAN networks enable us to modernize the whole education system. One of the most perspective ways of the modern educational system’s development is online education. Th...

Clarification of the Recent Scientific Approaches in Magnetic Water Treatment

The paper focused on study of influence magnetic water treatment (MWT) mechanism on physicochemical properties of aqueous solutions taking into account nature of changes in kinetics of chemical reactions. The theoretical...

Design and Analysis of Connecting Tie Rod Assembly for Automotive Application

The tie rod end is one of the most elementary parts of a steering mechanism, which has direct and crucial importance in terms of driving safety. The tie rod end is used to ensure that the wheels are aligned. It provides...

Analysis of Technogenic Load of Oil and Gas Production on Caspian Region

The problem of intensive pollution of the Caspian Sea has been continued to be one of the most significant and serious for the region. The rising of pollution level of the Caspian Sea coast with oil hydrocarbons has a pa...

Download PDF file
  • EP ID EP249328
  • DOI 10.21272/jes.2017.4(2).b11
  • Views 179
  • Downloads 0

How To Cite

H. A. A. Qazi (2017). Study of verification and validation of standard welding procedure specifications guidelines for API 5L X-70 grade line pipe welding. Журнал інженерних наук, 4(2), 11-14. https://europub.co.uk/articles/-A-249328