Surface Analysis Strategies for Conducting Polymers

Journal Title: Nanomedicine & Nanotechnology Open Access - Year 2017, Vol 2, Issue 1

Abstract

Recently, the utilisation of conducting polymers (CPs) has become ubiquitous in biomedical research due to their special properties. The processing simplicity of this type of polymers class was reported to be one of the main reasons behind its widespread scrutiny and application. In addition, their conductive properties may stimulate electrical signals for certain tissues such as the brain, nerve, and heart.

Authors and Affiliations

Mahat MM

Keywords

Related Articles

Recent Advances of Carbon Dot-Based Light-Emitting Diodes

Carbon dots (CDs), with abundant raw materials on earth, have become a new-type of luminescent materials and received great attention for their excellent merits such as low cost, low toxicity, strong photo stability, goo...

Physical Layer Considerations on Terahertz Networks

Terahertz band communication is attracting great interest and is expected to alleviate the capacity limitations of current wireless networks, and the upcoming 5G systems which incorporate millimeter wireless links but wo...

Nanoanesthesia - A Novel Approach to Local Anesthesia Drug Delivery

A technique using anesthesia containing nanoparticles, drawn to the targeted areaof body by magnets provide a useful alternative to nerve block for local anesthesia. This technique in patients suggests an experimental st...

Surface Analysis Strategies for Conducting Polymers

Recently, the utilisation of conducting polymers (CPs) has become ubiquitous in biomedical research due to their special properties. The processing simplicity of this type of polymers class was reported to be one of the...

Carbon nanotubes for "Ionic Wind" Craft or "Ionocraft"

Peter Thiel of the Founders Fund once famously said, "We wanted flying cars, and we got 140 characters."But nanotechnology now does make possible the long desired flying cars. It's a different propulsion method though th...

Download PDF file
  • EP ID EP282677
  • DOI 10.23880/nnoa-16000116
  • Views 103
  • Downloads 0

How To Cite

Mahat MM (2017). Surface Analysis Strategies for Conducting Polymers. Nanomedicine & Nanotechnology Open Access, 2(1), 1-2. https://europub.co.uk/articles/-A-282677