Computer system for casting defects classification based on Polish, French and Czech specifications

Journal Title: Archiwum Odlewnictwa - Year 2009, Vol 9, Issue 3

Abstract

Many foundries existing in Poland make casts for local and external market. It is necessary to adopt a quality control to client’s requirements. The main problem in the quality control of casting products is to detect and to classify properly defects. Polish defect classification is base nod the Polish Norm. In other countries (Czech Republic and France for example), other systems exist for classification, they are based on the different criteria and groups of defects. In other word the classification of casting defects is country-specific. Translation of defects names and their descriptions introduce additional level of difficulties. The authors propose multi-context system for finding equivalents of casting defects from one classification system to another, using original languages for each classification.

Authors and Affiliations

A. Adrian, J. Durak, B. Mrzygłód, S. Kluska-Nawarecka, K. Miłkowska, D. Wilk-Kołodziejczyk

Keywords

Related Articles

Selected characteristic of silumins with additives of Ni, Cu, Cr, Mo, W and V

The study, presents an investigation results of new grades of silumins containing of: 7,0÷17,0% Si, 4,0% Ni, 4,0% Cu and 0,5% Cr, Mo, W each as well as V. The influence tests were carried out of - antimony addition, stro...

Determination of Weibull Analysis of the Hypereutectic Silumins Reliability in Failure Time Respect

The results of dynamic evaluation of the reliability of hypereutectic AlSi17Cu3NiMg silumin under the effect of symmetrical cyclic tensile-compressive stresses were presented. Studies were carried out on a normal-running...

Heat resistance of Fe-Al intermetallics in the context of selected heat-resistant and hihg-temperature creep resistant steels

Results are hereby presented of heat-resistance tests of two Fe3Al and FeAl intermetallic phase-based alloys in the context of St41k-type boiler steel and 50H21G9N4 high-temperature creep resistant steel. It has been asc...

Thin wall ductile and austempered iron castings

It has been shown that it is possible to produce thin wall castings made of ductile iron with wall thickness in the range of 1.2 to 2.9 mm (without chills, cold laps and misruns). Thin wall ductile iron castings can be l...

Strength properties of moulding sands with chosen biopolymer binders

The article presents the results of primary researches of the IV generation moulding sands, in which as the binders are used different biodegradable materials. The bending and the tensile strength of the moulding sands w...

Download PDF file
  • EP ID EP71982
  • DOI -
  • Views 110
  • Downloads 0

How To Cite

A. Adrian, J. Durak, B. Mrzygłód, S. Kluska-Nawarecka, K. Miłkowska, D. Wilk-Kołodziejczyk (2009). Computer system for casting defects classification based on Polish, French and Czech specifications. Archiwum Odlewnictwa, 9(3), 5-8. https://europub.co.uk/articles/-A-71982