Enhancement in the Tribological and Mechanical Properties of Electroless Nickel-Nanodiamond Coatings Plated on Iron
Journal Title: Tribology in Industry - Year 2017, Vol 39, Issue 4
Abstract
A technology to improve the tribological and mechanical surface properties of iron alloys is developed based on the electroless nickel plating. The technology combines sol-gel and electroless deposition technique. Novel nanocomposite coatings are obtained consisting of Nickel-phosphorus-nanodiamond (Ni-P-ND). The ND sol is added directly to the electroless Ni-P solution. A suitable surfactant is added to achieve well-dispersed ND particles in the electroless solution to facilitate their embodiment and equal distribution in the coating. Substrates of steel 17CrNiMo6 and spheroidal graphite cast irons are used for the manufacture of the iron alloys specimens. The surface morphology and microstructure observation performed by scanning electron microscopy (SEM) and optical metallography confirms the influence of ND particles on the coating structure. The structural phase investigation by X Ray analysis indicates a transformation of the amorphous phase to a crystalline one such as Ni, Ni3P after coatings' heat treatment. The microhardness investigation by Knoop Method and wear resistance measurement in accordance with the Polish Standard PN-83/H-04302 of Ni-P and Ni-P-ND composite coatings are evaluated and compared with each other. The increase in the value of hardness and wear resistance of Ni-P composite coatings in the presence of ND particles and after heat treatment is obtained.
Authors and Affiliations
Z . Karaguiozova, J . Kaleicheva, V . Mishev, G . Nikolcheva
AFM Surface Roughness and Topography Analysis of Lithium Disilicate Glass Ceramic
The aim of this study is presenting AFM analysis of surface roughness of Lithium disilicate glass ceramic (IPS e.max CAD) under different finishing procedure (techniques): polishing, glazing and grinding. Lithium disilic...
Abrasive Wear Modes in Ball-Cratering Test Conducted on Fe73Si15 Ni10Cr2 Alloy Deposited Specimen
The objective of this study was to develop a theoretical model and associated wear mode map to identify the regimes in which two body abrasion (grooving abrasion) and three body abrasion (rolling abrasion) dominate in th...
Investigation of Wear Coefficient of Manganese Phosphate Coated Tool Steel
In recent years the properties of the coating in terms of wear resistance is of paramount importance in order to prevent the formation of severe damages. In this study, Wear coefficient of uncoated, Manganese Phosphate c...
Fracture Toughness and Tribological Wear Behaviour of Micro Alloyed Pearlitic- Ferritic Ductile Cast Iron
Fracture toughness and wear behaviour of micro alloyed ductile iron were investigated. Hardness, fracture, fracture toughness and wear tests were carried out on the ductile irons samples (D1, D2, D3, D4 and D5), containi...
Effect of Contact Temperature Rise During Sliding on the Wear Resistance of TiNi Shape Memory Alloys
The high wear resistance of TiNi shape memory alloys has generally been attributed to its pseudoelastic nature. In the present work the hardening effect due to its phase transformation from martensite to austenite due to...