ИССЛЕДОВАНИЕ ВЛИЯНИЯ АКТИВНОЙ МИНЕРАЛЬНОЙ ДОБАВКИ «ФОСФОЗОЛ» НА ПРОЦЕССЫ ГИДРАТАЦИИ И ФОРМИРОВАНИЯ МИКРОСТРУКТУРЫ КАМНЯ ПОРТЛАНДЦЕМЕНТА
Journal Title: INTERNATIONAL ACADEMY JOURNAL "Web of Scholar" - Year 2018, Vol 1, Issue 3
Abstract
The article presents the results of studies to determine the effect of phosphosol, a new type of active mineral additive in cement on the degree of hydration and formation of the microstructure of portland cement stone and the synthesis of its strength indexes
Authors and Affiliations
Г. Б. Бегжанова, М. И. Искандарова
ОЧИСТКА ОБЖИГОВОГО ГАЗА ЦЕМЕНТНОГО ПРОИЗВОДСТВА ПРИРОДНЫМИ ЦЕОЛИТАМИ
The industry faces the actual task of cleaning the waste gases from the kilns of cement production. Among the different methods of purification of gas systems adsorption methods acquire special importance, only adsorbent...
PERCEPTION GOTHIC CONCEPT IN THE WESTERN LITERATURE
This article observes the problem of importance and influence of Gothic culture in the international literary process.
WHO INTERNATIONAL CLASSIFICATION OF FUNCTION AS A DISABILITY DETERMINATION MODEL IN ARMENIA
WHO International Classification of Function focuses on the strengths of the individual, his saved capacities, contributing to its more active participation in public life and in work activities and thus can be implement...
ОХРАНА ОКРУЖАЮЩЕЙ СРЕДЫ В АГРАРНОЙ ЗОНЕ АЗЕРБАЙДЖАНА
As well as all countries of the world, Azerbaijan faces environmental problems of various character too. Uncontrollable use of means of chemicalization, pollution of water resources construction waters, pollution of atmo...
ПОКАЗНИКИ ТА РІВНІ РОЗВИТКУ ПРОФЕСІЙНОЇ ТВОРЧОСТІ БАКАЛАВРІВ ЛІСОВОГО І САДОВО-ПАРКОВОГО ГОСПОДАРСТВА: ВИЗНАЧЕННЯ КРИТЕРІЇВ
The article identifies and analyzes the criteria, indicators and levels of professional development of future bachelors of forestry and horticulture. The components, approaches to the development of professional creativi...