Metallic Matrix Composites with Ceramic Particles. Wetting Conditions

Abstract

The paper presents the main aspects regarding the mixtures obtained made up from aluminium melts and different kinds of ceramic particles (silicon carbide and boron carbide). Synthetically discussed are the wetting conditions and the wetting coefficient and the possibilities to improve it insisting on the alloying metal bath, its overheating and the heat treatment of the particles with the aim to remove gases from the superficial layer. The critical acceleration necessary for the incorporation of particles into the melt for different temperatures was determined.

Authors and Affiliations

G. NEAGU, Fl. ŞTEFĂNESCU, A. MIHAI, I. STAN

Keywords

Related Articles

Research on the Production of Sintered Powder 316

The 316 austenitic stainless steel powders are typically used in applications requiring good corrosion resistance, mechanical strength at high and very low temperatures, good ductility, wear resistance, associated in som...

The Quality of Metal Products Made on CNC Machines

Contemporary market must provide products that adapt to customer needs, which requires large investments and long-term employment. Producers have to take care of the buyers’ different way of thinking. The quality of prod...

Coatings Systems: Chromium Carbide, Nitride and Carbonitride

The process of the chemical deposition from vaporous implies the adsorption of the mobile atoms (monomers) on the substrate surface, their migration with embryos and stable nucleus formation, followed up by further growt...

Statistical Correlations Between Chemical Composition and Mechanical Properties of A516 Grade 65 Steel

In order to respond to required demands associated to certain operation conditions, the steels used in petroleum, petrochemical and chemical processing industries must have significant improved mechanical properties. The...

Mathematical Modelling of the Main Carburizing Thermochemical Treatment Parameters Influence on the Surface Hardness Parts Made in AMS 6265 (SAE 9310) Steel

This work is a part of broader experimental research study on the influence of the main process parameters (thermal, temporal and chemical of carburizing thermochemical treatment on the level of the main microstructural...

Download PDF file
  • EP ID EP596226
  • DOI -
  • Views 78
  • Downloads 0

How To Cite

G. NEAGU, Fl. ŞTEFĂNESCU, A. MIHAI, I. STAN (2013). Metallic Matrix Composites with Ceramic Particles. Wetting Conditions. Analele Universitatii "Dunarea de Jos" din Galati. Fascicula IX, Metalurgie si Stiinta Materialelor, 36(1), 38-41. https://europub.co.uk/articles/-A-596226