Results of Non-Destructive and Destructive Tests of Welded Joints Made of Heat-Resistant Cast Steel GX40NiCrSiNb35-25 in Welding Procedure Qualification
Journal Title: Biuletyn Instytutu Spawalnictwa - Year 2017, Vol 61, Issue 2
Abstract
The article presents test results concerning the welding procedure qualification of the production welding of heat-resistant cast steel GX40NiCrSiNb35-25 (1.4852) performed using filler metal WZ 25 35 Zr according to PN-EN ISO 14343. The welding procedure qualification test was performed in accordance with PN-EN ISO 11970. The test joint made using the TIG method (141) was subjected to non-destructive and destructive tests enabling the identification of the mechanical properties of the joint. The test results satisfied the requirements contained in PN-EN ISO 11970 and constituted the basis enabling the preparation of a related welding procedure qualification report.
Authors and Affiliations
Sławomir Parzych
Electron Beam Welding – Characteristics
The article presents the characteristics of electron beam welding and describes phenomena taking place during the interaction between an electron and an atom of a material being bombarded. The study also presents the bas...
Ultrasonic Tests of FSW Joints of Thicknesses Below 8 mm
The article presents results of ultrasonic tests concerning 6 mm thick FSW joints made of aluminium grade 2017. The tests were performed using joints with artificial post-weld welding imperfections and joints characteris...
Numerical Simulations of Modern Joining Techniques Illustrated with Examples of the FSW and EBW Methods
The article aims to present major advantages resulting from the use of tools for numerical analyses of modern welding processes, i.e. friction stir welding (FSW) and electron beam welding (EBW). The article presents basi...
Recent advances in fiber laser welding
Fibre lasers are innovative tools in the welder’s hands. The continuous development of fibre lasers combined with newly developed welding techniques enable the performance of technological tasks extremely difficult or ev...
Surfacing Performed Using Flux-Cored Wires in Ukrainian Companies
The article describes the experience of extending the service life of various machinery parts by surfacing them with flux-cored wires. High wear resistance during the rolling and straightening of steel is achieved by the...