The ATD thermal analysis of selected nickel superalloys

Journal Title: Archiwum Odlewnictwa - Year 2010, Vol 10, Issue 2

Abstract

The study presents the results of the ATD thermal analysis made on selected nickel alloys used by WSK Rzeszów for parts of aircraft engines. The aim of the studies was investigation of solidification parameters, especially Tlik and Tsol. The said parameters are very important in the determination of pouring temperature and maximum operating temperature of castings. Another important technical information is the quality of “master heat” ingots, examined for the stability of chemical composition and presence of different impurities. It has been concluded that the pouring temperature of CMSX-4 and MAR-247 alloys should be comprised in a range from 1470 to 1480°C, while for the remaining alloys the recommended range of pouring temperatures is from 1440 to 1450°C. Examinations have also proved that some batches of the supplied ingots are contaminated with non-metallic impurities, located mainly in the region of shrinkage cavities.

Authors and Affiliations

F. Binczyk, J. Śleziona

Keywords

Related Articles

Analysis of the failure causes in an element made of AlSi11Cu2(Fe) alloy

The paper presents results of research on a cross element damaged during the service, made of the casting alloy of aluminum - AlSi11Cu2(Fe) (AK132). Performed research was to explain the reasons for this damage and inclu...

Influence analysis foamed polystyrene model on casting defects as well as microstructure ductile cast iron from Lost Foam process with Inmold method

In this work was shown a influence analysis foamed polystyrene model on casting defects as well as microstructure ductile cast iron from Lost Foam process with Inmold method.

Preliminary Research on Granulation Process of Dust Waste from Reclamation Process of Moulding Sands with Furan Resin

The results of investigations of the granulation process of foundry dusts generated in the dry mechanical reclamation process of used sands, where furan resins were binders are presented in the paper. Investigations conc...

Trials to manufacture and test castings from Inconel alloy

The article describes the methods of producing and testing the Inconel 740 nickel alloy in as-cast state. An assumption has been made that the obtained alloy should be characterised by a normative chemical composition an...

Selected aspects of the piece production of iron alloy castings in terms of their environmental impact

Problems of environmental protection are nowadays one of the top priorities in a policy programme adopted by the European Community. Reducing the negative impact of the domestic foundry industry on environment should res...