Abstract
Selected slewing bearings and their application have been described in this article. Basic causes of the damage pitch surfaces of slewing bearings have been analyzed and examples of the damage have been presented as well. Special attention was paid to these kinds of damage which appeared most often in the case of the pitch surfaces of the bearings and those ones which very often cause premature exchange of the bearing and its scrapping. On the basis of the conducted studies it was stated that the main cause of the damage to the pitch surfaces of the bearings is the excessive load of rolling elements. Based on the results of the conducted analysis, actions limiting the occurrence of the damage to the pitch surfaces of the bearings, which lead to their premature exchange, have been proposed. One of the suggested actions, limiting the premature exchange of bearings, is the necessity of exceptionally thorough design and selection of the slewing bearings, including the conditions of their foundation.
Authors and Affiliations
Marek Krynke, Jacek Selejdak, Stanislaw Borkowski
Influence of process parameters on torsional strength, impact toughness and hardness of dissimilar AISI 304 and AISI 1021 friction welded steels
In this present study an attempt was made to join austenitic stainless steel (AISI 304) with low alloy steel (AISI 1021) at different rotational speeds and at different axial pressures and then determining the strength o...
Mechanical properties of homogenized twin-roll cast and conventionally cast AZ31 magnesium alloys
The improvement of mechanical properties of magnesium alloys nowadays is very important, because of the variety of industrial applications. For this goal, the number of casting techniques and further treatments were deve...
Microstructural changes of AISI 316L due to structural sensitization and its influence on the fatigue properties
Mechanical and fatigue properties of material are dependent on its microstructure. The microstructure of AISI 316L stainless steel commonly used for the production of medical tools, equipment and implants can be easily i...
[sub][/sub][sub][/sub]PROPERTIES OF PLASMA AND HVOF SPRAYED COATINGS
The article compares the properties of plasma and HVOF thermally sprayed coatings obtained by blending the NiCrBSi and Fe2O3 powders. The deposition was performed by means of the Plancer PN-120 and the Diamond Jet guns f...
FRACTURE BEHAVIOUR OF P/M Cr-V LEDEBURITIC STEEL WITH DIFFERENT SURFACE ROUGHNESS
The samples made from the Vanadis 6 PM ledeburitic tool steel were surface machined to different quality and heat treated by standard regime of the processing. Three point bending tests were carried out on processed samp...