This work presents research into properties of the surface layer of the C45 steel following the treatment with highly-focused thermal stream utilizing the GTAW method. The remelting of the surface layer of the sample was performed using welding head moving with a constant speed of 200 mm/min with the amperage of the electrical arch ranging from 50 to 300A. The fractographic measurements of the tested fractures were performed using the SEM microscope. A relationship was established between the current amperage and the speed of the movement of the welding head versus the type of the fractures.

Authors and Affiliations

S. Adamiak

Keywords

Related Articles

Weld microstructure in cast AlSi9/SiC(p) metal matrix composites

Welded joint in cast AlSi9/SiC/20(p) metal matrix composite by manual TIG arc welding using AlMg5 filler metal has been described in his paper. Cooling curves have been stated, and the influence in distribution of reinfo...

The influence of modification and squeeze casting on properties of AlSi11 alloy castings

The results of structural examinations and tests of mechanical properties of AlSi11 alloy, either gravity or squeeze cast, have been presented. The investigations have been carried out for both the non-modified silumin a...

The Lost Foam method – pre-expansion process

In the study, a pre-expansion station, designed by authors, was presented. It consists of a batch pre-expander with a 90 liters capacity foaming chamber, equipped with fluidized-solid dryer of pre-expanded beads and a pn...

Effect of ring notch radius on the decohesion mode in AlSi alloys

The article discusses the effect of the, determined by tensile test, non-linear characteristics of AlSi alloys on the value of the shape factor k for the three different sizes of the radius of the ring notch made on roun...

Effect of additions of Cr, Mo, W and/or Si on the technological properties of aluminum-iron-nickel bronze

The aim of this study was to investigate the effect of additives of Cr, Mo, W and / or Si CuAl10Fe5Ni5 bronze, cast into sand moulds, the bronze technological properties such as: porosity, volumetric shrinkage Sv, linear...

Download PDF file
  • EP ID EP72291
  • DOI -
  • Views 82
  • Downloads 0

How To Cite

S. Adamiak (2011). Fractographic research of the C45 steel remelted with a plasma of electric arc. Archiwum Odlewnictwa, 11(3), 39-42. https://europub.co.uk/articles/-A-72291