Abstract
Sintering is the most important process where iron ore fines are converted into a suitable lumpy product for blast furnace consumption. In this study, received sinter from Vizag Steel Plant, India has been used. The solid state isothermal reduction kinetics has been carried out using coke dust (treated as industrial waste) as reductant at temperature 1373K over a period of time from 5 to 90 minutes. The chemical analyses have been performed to get the degree of metallization of the reduced sinters and these data are used as input for the determination of the best fitted kinetic model. The characterizations of the reduced sinters are analyzed by XRD. The reduction mechanism is found to be contracting geometry
Authors and Affiliations
ARGHYA MAJUMDER, BITAN KUMAR SARKAR, MAHARSHI GHOSH DASTIDAR, GOPES CHANDRA DAS, RAJIB DEY
Critical Factors Responsible for Failure of Construction Project in Kolkata: an Empirical Study
Priority should be given to the rapidly changing construction industry in India in order to meet the challenges associated with the infrastructure projects management. This study has been performed for identifying the fa...
Effect of Heat Treatment on Al2024 Reinforcement With Multiwalled Carbon Nanotube
In this research paper, Multiwalled carbon nanotubes (MWCNTs) reinforced with Al2024 were ball milled for homogenization of powder. Nanocomposite was developed using MWCNT reinforcement having 0.5%, 1.5%, and 2.5% weight...
Effect of Carburization on the Mechanical Properties of EN-8 Steel in different Quenching Medium at different Quenching Time Intervals
EN-8 is widely used for many general engineering applications. Typical applications include shafts, studs, bolts, connecting rods, screws, rollers. The Main Purpose of the Paper is to study the effect of heat treatment o...
Dependence Parameters on Dielectric Behavior of Mo6+ Substituted Lithium Ferrites
High variance Mo6+ substituted lithium ferrite with general formula [Li (1+3y)/2MoyFe2.5-5y/2] O4: where y=0.05 to 0.5 in steps of 0.05 were prepared under solid- state reaction method sintered at high temperature 1200o...
Microstructure Analysis of Genuine Copper Alloy Coin
Coin characterization analysis (coins) is done by using the test method such as; Spectrometer XRF, XRD Defractometer, Deferential Scanning Calorimeter, Scanning Electron Microscope (SEM). Characterization is done in Lab...