Abstract

Definition of a composite [1] describes an ideal composite material with perfect structure. In real composite materials, structure is usually imperfect – composites contain various types of defects [2, 3–5], especially as the casted composites are of concern. The reason for this is a specific structure of castings, related to course of the manufacturing process. In case of metal matrix composite castings, especially regarding these manufactured by saturation, there is no classification of these defects [2, 4]. Classification of defects in castings of classic materials (cast iron, cast steel, non-ferrous alloys) is insufficient and requires completion of specific defects of mentioned materials. This problem (noted during manufacturing metal matrix composite castings with saturated reinforcement in Institute of Basic Technical Sciences of Maritime University Szczecin) has become a reason of starting work aimed at creating such classification. As a result, this paper was prepared. It can contribute to improvement of quality of studied materials and, as a consequence, improve the environment protection level.

Authors and Affiliations

K. Gawdzińska, D. Nagolska, M. Szweycer

Keywords

Related Articles

Elements of the efficiency system improvement of foundry

The effectiveness of industrial systems is being ranked among important factors industrial engineering in foundry. He determines internal production abilities of foundry. It is possible to describe the effectiveness the...

Efficiency of protective coatings on high creep resistant cast steel

This paper presents results of research of multilayer aluminium–silicon coatings. Aluminium–silicon coatings were created on high– temperature creep resist cast iron using slurry method in air atmosphere. These coatings...

Maintenance system improvement in cast iron foundry

The work presents the issue of technical equipment management in an iron foundry basing on the assumptions of the TPM system (Total Productive Maintenance). Exploitation analysis of automatic casting lines has been carri...

Residual stress state in titanium alloy remelted using GTAW method

Test materials comprised two-phase titanium alloy Ti6Al4V (Grade5). The surface of the tested alloy was remelted by means of TIG welding method using variable current-voltage parameters. The investigations aimed to deter...

The modification process of AlSi21CuNi silumin and its effect on change of mechanical properties of the alloy

Due to difficulties present during machining operations and with segregation of crystals of primary silicon, hypereutectic silumins can be used after modification only. It is why elaboration of effective modification met...

Download PDF file
  • EP ID EP72687
  • DOI 10.2478/v10266-012-0077-y
  • Views 104
  • Downloads 0

How To Cite

K. Gawdzińska, D. Nagolska, M. Szweycer (2012). Classification of Structure Defects of Metal Matrix Castings with Saturated Reinforcement. Archiwum Odlewnictwa, 12(3), 29-36. https://europub.co.uk/articles/-A-72687